Chinese | English

厂家logo
E-MAIL:15230713671@163.com           TEL:0086-17761570021
    ELBOW MACHINE
    Current position: HOME> Mechanical equipment>

    Medium and small carbon steel elbow machine

    Medium and small carbon steel elbow machine

    Mechanical parameters

    Hot forming elbow machine

    Processing rangel

    1”—6”

    3”—12”

    8”—24”

    16”—30”

    20”—36”

    30”—48”

    32”—56”

    MAX.wall thickness

    Sch40

    MAX.pressure

    31.5MPa

    Working pressure

    25 MPa

    Working speed

    0—1000mm/min

    Return speeed

    1500—2000mm/min

    Cylinder diameter

    125mm*2

    180mm*2

    300mm*2

    320mm*2

    360mm*2

    280mm*4

    320*4

    Cylinder Stroke

    3000mm

    4000mm

    5000mm

    5000mm

    6000mm

    8000mm

    10000mm

    Cylinder thrust

    30T*2

    30T*2

    175T*2

    200T*2

    250T*2

    150T*4

    200T*4

    Motor power

    18.5kw

    22.5kw

    37.5kw

    48kw

    56kw

    68kw

    80kw

    IF Power supply needed

    160kwa

    250kwa

    400kwa

    500kwa

    600kwa

    800kwa

    1000kwa

     

     

     

     

     

     

    Mechanical video

    Equipment details

    The forming process of hot push elbow machine is based on the working principle of using special medium frequency induction elbow machine, elbow push machine, core die and heating device to make the steel pipe and tube blank on the die move forward under the push of push machine, and be heated, enlarged and bent in the movement. Notes for elbow making: the diameter of pipe blank must be smaller than that of elbow, otherwise it will affect the wall thickness requirements of forming elbow. Reason is due to the deformation characteristics of the hot pushing elbow is according to the volume before and after plastic deformation rule of metal materials determine the pipe diameter, adopted by the medium frequency pipe billet diameter less than bend diameter of bend machine, through the core module and control the deformation of the process, make the inner arc compressed metal flow, the compensation to other parts of the thinned by hole diameter, wall thickness uniform Angle is obtained.